1.4313
EN/DIN
DIN/EN 10272
INT
X3CrNiMo 13-4
EN 1.4313 round stainless steel is a martensitic stainless steel formulated for primary forming in forged products. 1.4313 is the EN numerical designation for this material. X3CrNiMo13-4 is the EN chemical designation.
This material is well established: A number of published standards are identified in the Further Reading section below and this list is not necessarily exhaustive.
It has a moderately high base cost among the forged martensitic stainless steels in the database.
Electrical Properties
Electrical Resistance
|
0.60 x10 ^ -6 Ω .m
|
Thermal conductivity
|
25 W/m-K
|
Maximum Temperature: Corrosion
|
390℃
|
Process Properties
Machinability
|
good
|
Hot Forming
|
good
|
Hardness HB
|
242
|
Thermal Recovery
Specific heat capacity
|
480 J/kg-K
|
Melting point
|
1450℃
|
1.4313 yuvarlak paslanmaz çelik sınıfı ayrıca aşağıdaki tanımlamalara karşılık gelir:
X3CrNiMo13-4,AISI CA6-NM, UNS S41500, SGS6X, JIS SCS5, ASTM A182 F6NM, SS 2384, B.S. 425C11, AFNOR Z4CND13.4M
|
Dimensions mm |
X3CrNiMo 13-4 |
10 |
up to |
325 |
Chemical Composition
Grade |
C |
Cr |
Mn |
P |
Si |
S |
Mo |
Ni |
1.4313
|
0.05 max |
14 max
|
1.5 max |
0.04 max |
0.7 max |
0.015 max |
0.7
max
|
0.02 max |
Physical Composition
It is used in the construction of power plant, electricity generation, pumps, compressors and turbine wheels.
Density
g/cm3
|
Specific heat capacity J/kg K |
Thermal conductivity W/m K |
Electrical resistivity
Ω mm2/m
|
7.7
|
430 |
25 |
0.6
|
Hardness HB 30
≤ HB
|
0.2%Yield Strength R ≥
N/ mm2
|
Tensile strength R N/ mm2
|
Elongation A ≥ %
|
Modulus of elasticity
kN/mm2
|
320
|
520
|
700-800
|
15/12
|
200
|