Product \ Round \ Martensitics \ 1.4029

1.4029

EN/DIN

X29CrS13

Electrical Properties

Electrical Resistance

0.60 x10 ^ -6 Ω .m

Thermal conductivity

30 W/m-K

Maximum Temperature: Corrosion

390℃

 

Process Properties

Machinability

good

Hot Forming

good

Hardness HB

424

 

Thermal Recovery

Specific heat capacity

480 J/kg-K

Melting point

1440℃

  Dimensions  mm
X29CrS13 10 up to 350

 

Chemical Composition

Grade C Cr Mn P Si S Mo

1.4029

0.32 max

18 max

1.5 max 0.40 max 1.0 max 0.025 max

0.60

max

 

Physical Composition

It is used in the construction of power plant, electricity generation, pumps, compressors and turbine wheels.

 

Density

g/cm3

Specific heat capacity J/kg K Thermal conductivity W/m K

Electrical resistivity 

Ω mm2/m

7.7

541 32.3

0.6

 

Hardness HB 30

≤  HB

0.2%Yield Strength R ≥

 N/ mm2

Tensile strength R N/ mm2

Elongation A ≥ %

Modulus of elasticity

kN/mm2

320

520

428

31

200